This is a 3mf with the settings I use to print PA6-CF and PA6-GF on my Bambu P1s.
Requires Hardened Extruder Gears and Hardened Nozzle.
I dry my material for 12-24 hours at 70c With a SUNLU SP2 and continue to dry throughout the entire print.
Supports may need to be painted on depending on object and orientation.
Try to avoid large flat surfaces on the build plate to prevent warping.
.22 Muzzle device included to show recommended orientation.
HUUUGE Shoutout to Unseenkiller for showing me where to get started with nylons.
LBRY Tags: 3d2a; guncad